Abstract
This study investigates the impact of high-pressure hydrogen gas exposure on the structural and morphological characteristics of O-ring materials. O-ring specimens undergo two cycles of sealing under 70 MPa hydrogen gas, and their resulting variations are examined using advanced characterization techniques, including powder X-ray diffraction (PXRD), small-angle X-ray scattering (SAXS), scanning electron microscopy (SEM) and atomic force microscopy (AFM). Our findings reveal that the lattice parameters of the O-ring material show no significant changes when exposed to 70 MPa hydrogen gas. However, in the micrometre range, the formation of a hierarchical channel morphology becomes evident. This morphology is accompanied by the separation of carbon black filler from the rubber matrix, contributing to mechanical weakening of the O-ring. These observations can be attributed to the pressure gradient that develops between the inner and outer radii of the O-ring, resulting from compression forces acting perpendicularly to the radial direction due to clamp locking.
| Original language | English |
|---|---|
| Article number | 5319 |
| Journal | Scientific Reports |
| Volume | 14 |
| Issue number | 1 |
| DOIs | |
| Publication status | Published - Dec 2024 |
Bibliographical note
Publisher Copyright:© The Author(s) 2024.
Fingerprint
Dive into the research topics of 'Hierarchical channel morphology in O-rings after two cycling exposures to 70 MPa hydrogen gas: a case study of sealing failure'. Together they form a unique fingerprint.Cite this
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver