Self-assembled growth and luminescence of crystalline Si/SiOx core-shell nanowires

S. Kim, C. O. Kim, D. H. Shin, S. H. Hong, M. C. Kim, J. Kim, S. H. Choi, T. Kim, R. G. Elliman, Y. M. Kim

Research output: Contribution to journalArticlepeer-review

12 Citations (Scopus)

Abstract

Crystalline Si/SiOx core/shell nanowires(NWs) are self-assembled by annealing Ni-coated hydrogenated Si-rich SiOx (SRO:H) films at 1100 °C in the presence of Si powder. Plasma-enhanced chemical vapor deposition is used to grow 100nm SRO:H thin films with varying silicon concentration (nSi). The NWs vary from SiOx nanowires to Si/SiOx core/shell structures depending on the composition of the SRO:H substrate, with the fraction of core/shell structures increasing with increasing Si concentration. As nSi increases from 37 to 43at.%, the average diameter of the NWs also increases from 48 to 157nm. A growth model based on the diffusion-assisted vapor-liquid-solid mechanism is proposed to explain how the core/shell structures are self-assembled. Photoluminescence(PL) spectra of the individual NWs have two major emission bands in the near UV (381nm) and blue (423nm) ranges at nSi = 43at.%, named as UV and BL PL bands, respectively. In contrast, only the BL PL band is observed at n Si ≤ 39at.%. These results suggest that the BL and UV PL bands can be attributed to the defect states in the SiOx shell and at the Si core/SiOx shell interface, respectively, and that the BL band is closely related to the growth process of the NWs.

Original languageEnglish
Article number205601
JournalNanotechnology
Volume21
Issue number20
DOIs
Publication statusPublished - 2010