Water resistance of three biopolyester films, such as poly-L-lactate (PLA), poly-hydroxybutyrate-co-valerate (PHBV), and Ecoflex, and low density polyethylene (LDPE) film was investigated by measuring contact angle of various probe liquids on the films. The properties measured were initial contact angle of water, dynamic change of the water contact angle with time, and the critical surface energy of the films. Water contact angle of the biopolyester films (57.62-68.76°) was lower than that of LDPE film (85.19°) indicating biopolyester films are less hydrophobic. The result of dynamic change of water contact angle also showed that the biopolyester films are less water resistant than LDPE film, but much more water resistant than cellulose-based packaging materials. Apparent critical surface energy for the biopolyester films (35.15-38.55 mN/m) was higher than that of LDPE film (28.59 mN/m) indicating LDPE film is more hydrophobic.

Original languageEnglish
Pages (from-to)234-237
Number of pages4
JournalFood Science and Biotechnology
Volume16
Issue number2
Publication statusPublished - 2007

Keywords

  • Biopolyester film
  • Contact angle
  • Surface tension
  • Thermo-compression
  • Wetting property

Fingerprint

Dive into the research topics of 'Wetting properties of biopolyester films prepared by thermo-compression method'. Together they form a unique fingerprint.

Cite this